Differential Scanning Calorimetry (DSC)

1 2009 TA InstrumentsDifferential Scanning CalorimetryBasic Theory & Applications Training (DSC) DSC Training CourseAgenda Understanding DSC Experimental Design Calibration Optimization of DSC Conditions Interpretation of Undesirable Events in DSC Data Applications2 DSC Training Course2900 Series DSC sDSC 2010 DSC 2910 DSC 2920 DSC Training CourseQ1000Q100Q10 First Generation Q Series DSCs3 DSC Training CourseSecond Generation DSCsQ2000Q200 AutoQ20Q2000 is top of the line, research grade with all optionsQ200 is research grade and expandableQ20 is a basic DSC Available as an Auto Q20 & also Q20 PDSC Training CourseUnderstanding DSC.

Endothermic Heat Flow Heat flows into the sample as a result of either Heat capacity (heating) Glass Transition (T g) Melting Evaporation Other endothermic processes Endothermic DSC Training Course-0.1 0.0 0.1 Heat Flow (W/g) 0 20 40 60 80 100 120 140 160 Exo Up Temperature (°C) Exothermic Heat Flow Heat flows out of the sample as a result of ...

Loading..

Tags:

  Endothermic, Exothermic, Endothermic dsc

Information

Domain:

Source:

Link to this page:

Please notify us if you found a problem with this document:

Spam in document Broken preview Other abuse

Transcription of Differential Scanning Calorimetry (DSC)

Related search queries