PPD-407B Injection Molding Troubleshooting Guide …

Injection moldingTroubleshooting guideEastman copolyestersBlack specks .. 3 Brittleness .. 3 Discoloration .. 4 Flashing .. 4 Flash and short shot in different shots .. 5 Flash and short shot in the same shot .. 5 Flowlines vs . seagulls, hooks, heat marks .. 6 Gate blush ..07 Haziness ..07 Hot runners, hot sprues, valve gates .. 08 Jetting .. 08 Sinks and voids .. 08 Splay ..09 Air splay and decompression splay .. 09 Contamination splay .. 09 Heat splay .. 10 Moisture splay ..10 Shear splay .. 11 Other splay .. 11 Sprue sticking ..12 Unmelts .. 12 Warped or distorted parts as ejected from the mold ..13 Warped parts after packing/shipping.

Possible cause Corrective action Previous material(s) in the screw, check ring, hot runner, etc . Purge machine with Eastman™ copolyesters or commercial purge compounds .

Loading..

Tags:

  Machine, Injection

Information

Domain:

Source:

Link to this page:

Please notify us if you found a problem with this document:

Spam in document Broken preview Other abuse

Transcription of PPD-407B Injection Molding Troubleshooting Guide …

Related search queries