5 Physical propertiesELASTOLLAN PHYSICAL PROPERTIESM echanical propertiesThe physical properties of Elastollan are discussed below. The test procedures are explained in some detail. Typical values of these tests are presented in our brochure Elastollan Product Range and in separate data are carried out on injection molded samples using granulate which is pre-dried prior to processing. Before testing specimens are conditioned for 20 hours at 100 C and then stored for at least 24 hours at 23 C and 50 % relative humidity. The values thus obtained cannot always be directly related to the properties of finished parts.
calorimetry (DSC) at a heating rate of 10 K/min. The Tg was evaluated according to DIN EN ISO 11357-2 on the basis of the curve, the slope of which is stepped in the transition range. The torsion modulus and the damping curves shown in figs. 8 to 13 enable Tg’s to be defined on the basis of the damping maximum. Since this is a
Domain:
Source:
Link to this page:
Please notify us if you found a problem with this document:
{{id}} {{{paragraph}}}