Undercooling related casting defects in single

Found 1 free book(s)
Undercooling Related Casting Defects in Single …

Undercooling Related Casting Defects in Single

www.tms.org

UNDERCOOLING RELATED CASTING DEFECTS IN SINGLE CRYSTAL TURBINE BLADES M. Meyer ter Vehn, D. Dedecke, U. Paul* and P.R. Sahm GieBerei-Institut, RWTH Aachen, Intzestr.