Die Casting Defects Causes and Solutions - Runner …

Die Casting Defects Causes and Solutions - Runner …

Back to document page

Solutions : Inspect the ways how gas is drawn into the metal melts flow or inspect whether the gas is from the air, the steam, the mold lubricant etc.