04543 - STRESS CORROSION CRACKING IN FUEL ETHANOL: …
www.icorr.netSTRESS CORROSION CRACKING IN FUEL ETHANOL: A NEWLY RECOGNIZED PHENOMENON R.D. Kane and J.G. Maldonado InterCorr International, Inc. 14503 Bammel North Houston Road, Suite 300