Transcription of 316L Grade Stainless Steel (1.4404 to EN 10088)
1 316L Grade Stainless Steel ( to EN 10088). Material: Austenitic Stainless Steel . Metallurgical composition: 17% Cr. / 11% Ni. / 2% Mo. Tensile Strength N/mm : 530 Minimum. Proof stress N/mm: 240 Minimum. Elongation %: 40 Minimum. Finishes: natural or electro-chemical polish. Applications: Marine Grade , high corrosion resistance suitable for salt laden environments onshore & offshore. For internal and external locations with good impact resistance for type 4X enclosures. Used extensively in food processing industries due it's superior material properties.
2 304 Grade Stainless Steel ( to EN 10088). Material: Austenitic Stainless Steel . Metallurgical composition: 18% Cr. / Ni. Tensile Strength N/mm : 520 Minimum. Proof stress N/mm: 230 Minimum. Elongation %: 45 Minimum. Finishes: Electro-chemical polish or Painted, Polyester epoxy powder coating. Applications: Good corrosion resistance suitable for non-salt laden environments onshore. For internal and external locations with good impact resistance for type 4X enclosures. 400 Series Stainless Steel ( to EN 10088). Material: Ferritic Stainless Steel . Metallurgical composition: 11% Cr.
3 + Ti. Tensile Strength N/mm : 380 Minimum. Proof stress N/mm: 220 Minimum. Elongation %: 25 Minimum. Finishes: Painted, Polyester epoxy powder coating. Applications: Corrosion resistance suitable for non-salt laden environments onshore. For internal and external locations with good impact resistance for type 4X enclosures