DescriptionGMAW wire for % Mo alloyed boiler, plate and tube steels as well as in pressure vessel andstructural steel engineering. Highly-quality, very tough deposit of high cracking resistance, non-ageing. Approved in long-term condition up to +550 C service temperature, low temperaturetoughness to -40 C. The wire shows good feeding and welding characteristics, resulting insmooth welding and wetting behaviour. Uniform copper bonding with low total copper and CertificatesT V-D (0021.), DB ( ), Z ( ), BB, T V-A (76), CL (0216), FI (G MoSi),UDT, SEPROZSame Alloy Filler MetalsSMAW stick electrode: FOX DMO KbSAW combination:EMS 2 Mo/BB 24 FOX DMO TiEMS 2 Mo/BB 25 GTAW rod:DMO-lGGas welding rod:DMOBase Materialshigh temperature steels and similar alloyed cast steels, ageing resistant and steels resistantto caustic cr

Description GMAW wire for 0.5 % Mo alloyed boiler, plate and tube steels as well as in pressure vessel and structural steel engineering. Highly-quality, very tough deposit of high cracking resistance, non-

Tags:

  Miso, G mosi aws a5

Information

Domain:

Source:

Link to this page:

Please notify us if you found a problem with this document:

Other abuse

Transcription of EN 12070:1999: G MoSi AWS A5.28-96: ER70S-A1 (ER80S-G ...

1 DescriptionGMAW wire for % Mo alloyed boiler, plate and tube steels as well as in pressure vessel andstructural steel engineering. Highly-quality, very tough deposit of high cracking resistance, non-ageing. Approved in long-term condition up to +550 C service temperature, low temperaturetoughness to -40 C. The wire shows good feeding and welding characteristics, resulting insmooth welding and wetting behaviour. Uniform copper bonding with low total copper and CertificatesT V-D (0021.), DB ( ), Z ( ), BB, T V-A (76), CL (0216), FI (G MoSi),UDT, SEPROZSame Alloy Filler MetalsSMAW stick electrode: FOX DMO KbSAW combination:EMS 2 Mo/BB 24 FOX DMO TiEMS 2 Mo/BB 25 GTAW rod:DMO-lGGas welding rod.

2 DMOBase Materialshigh temperature steels and similar alloyed cast steels, ageing resistant and steels resistantto caustic cracking16Mo3, S355J2G3, L320 - L415NB, L320 MB - L415MB, P255G1TH, P235GH, P265GH,P295GH, P310GH, P255NH, 17 MnMoV6-4, 22 NiMoCr4-7, 20 MnMoNi5-5, 15 NiCuMoNb5,20 MnMoNi4-5, GE240-GE300, 22Mo4, S255N - S460N, P255NH-P460 NHASTM A335 Gr. P1; A161-94 Gr. T1 A A182M Gr. F1; A204M Gr. A, B, C; A250M Gr. T1;A217 Gr. WC1 Operating Datashielding gases: mmArgon + 15 - 25 % % , interpass temperature and post weld heat treatment as required by the base Properties of All-weld Metal(*) u u2ayield strength ReN/mm2: 500( 470)470( 450)450( 400)tensile strength RmN/mm2: 620( 550)590( 520)570( 515)elongation A (L0= 5d0) %: 25( 322)23( 320)25( 419)impact work ISO-V KV J+ 20 C:150( 120)160150( 120)- 40 C.

3 ( 347)( 347)(*) u untreated, as-welded - shielding gas Ar + 18 % CO2u2 untreated, as-welded - shielding gas 100 % CO2a annealed, 620 C/1 h/furnace down to 300 C/air shielding gas Ar + 18 % CO2 Typical Composition of Solid WireCSiMnMowt-% 12070:1999: G MoSiAWS : ER70S-A1 (ER80S-G) HLER DMO-IGGMAW solid wire, low-alloyed, high temperature2-140 High Temperature and Creep-resistant Filler Metals GMAW Solid Wir