KOBE STEEL's High Performance Copper Alloy Strips for Terminals and Connectors.. KFC KLF -2 KLF -5 CAC 5 . Alloys CAC 16 CAC 19 CAC 60 CAC 75. Properties CDA No. C19210 - C50715 C19040 C19800 C19419 C64760 - Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Fe Fe Fe Ni Fe Fe Ni Ni wt% P P P P P Si Si Si Chemical Compositions (Nominal) Sn Sn 2 Sn Zn Zn Zn Zn 1. Sn Sn Sn Sn Mg Mg . Specific Gravity Physical Properties 293 573K -6. 10 /K Temper SP Typical Coefficient of Thermal Expansion . W/m K 364 318 150 166 Temper SP 247 254 197 166.

神戸製鋼の端子・コネクタ用高性能銅合金板条 KOBE STEEL's High Performance Copper Alloy Strips for Terminals and Connectors.

Information

Domain:

Source:

Link to this page:

Please notify us if you found a problem with this document:

Other abuse

Advertisement

Transcription of 神戸製鋼の端子・コネクタ用高性能銅合金板条 - KOBELCO

1 KOBE STEEL's High Performance Copper Alloy Strips for Terminals and Connectors.. KFC KLF -2 KLF -5 CAC 5 . Alloys CAC 16 CAC 19 CAC 60 CAC 75. Properties CDA No. C19210 - C50715 C19040 C19800 C19419 C64760 - Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Cu Rem. Fe Fe Fe Ni Fe Fe Ni Ni wt% P P P P P Si Si Si Chemical Compositions (Nominal) Sn Sn 2 Sn Zn Zn Zn Zn 1. Sn Sn Sn Sn Mg Mg . Specific Gravity Physical Properties 293 573K -6. 10 /K Temper SP Typical Coefficient of Thermal Expansion . W/m K 364 318 150 166 Temper SP 247 254 197 166.

2 Thermal Conductivity . n m Temper SP Electrical Resistivity . %IACS 90 80 35 40 Temper SP 61 63 44 40. Electrical Conductivity . GPa 125 127 123 130 118 120 127 127. Modulus Elasticity . Poisson's ratio . MPa 295 370 330 min 365 450. Tensile Strength Mechanical Properties . 15 min 13 min 15 min Temper 1/4H Elongation . MHv: 85 110 80 120 90 140. Vickers Hardness . MPa 350 430 440 540 335 470. Tensile Strength . 4 min 8 min 8 min Temper 1/2H Elongation . MHv: 100 130 140 180 100 150. Vickers Hardness . MPa 390 470 390 min 530 640 500 590 450 550 470 580 600 700 700 850.

3 Tensile Strength .. Temper H 2 min 7 min 5 min 7 min 5 min 5 min 10 min 5 min (H/SP CAC5) Elongation . MHv: 120 145 120 160 160 200 155 185 130 170 140 175 180 220 210 260. Vickers Hardness . MPa 590 min 540 630 640 740. Tensile Strength .. Temper EH - 5 min 3 min EH/SP CAC5 Elongation . MHv: 180 min 165 200 190 230. Vickers Hardness