Material Specification SheetDISOGRIN 6865 Name:DISOGRIN 6865 Material : Premium polyurethane, TODI basedType:Injection moldedColor:NaturalPropertyStandardValue UnitsImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory Spec Sheet 6865 D-2240-6892 Shore ATensile StrengthASTM D-412 Die C5,900psiElongation SetASTM D-412 Die C550%Elongation SetASTM D-412 Die C15%300% ModulusASTM D-412 Die C1,700psi100% ModulusASTM D-412 Die C750psiAbrasion LossDIN 53/51625mm3 Tear Die CASTM D-624660pliTear NickedASTM D-624360pliBayshore ResilenceASTM D-2632-751%Compression Set B 22 Hrs @ 70 CASTM D-395-69, Method B 9%Specific GravityASTM D-792, Method Specification SheetDISOGRIN 9250 PropertyStandardValueUnitsHardnessASTM D-2240-6892 Shore ATensile StrengthASTM D-412 Die C6,000psiElongation SetASTM D-412 Die C400%Elongation SetASTM D-412 Die C18%300% ModulusASTM D-412 Die C3,400psi100% ModulusASTM D-412 Die C1,600psiAbrasion LossDIN 53/51636mm3 Tear Die CASTM D-624700pliTear NickedASTM D-624480pliBayshore ResilenceASTM D-2632-735%Compression Set22 Hrs @ 70 CASTM D-395-69 (Method B)26%Specific GravityASTM D-792, Method.

Material Specification Sheet DISOGRIN D80S Hardness ASTM D-2240 85 ± 3 Shore A Tear Strength ASTM D-624 67 N/mm, Min. Tensile Strength ASTM D-412 25 MPa, Min.

Tags:

  Specification, Astm

Information

Domain:

Source:

Link to this page:

Please notify us if you found a problem with this document:

Other abuse

Transcription of Material Specification Sheet - industrialseal.com

1 Material Specification SheetDISOGRIN 6865 Name:DISOGRIN 6865 Material : Premium polyurethane, TODI basedType:Injection moldedColor:NaturalPropertyStandardValue UnitsImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory Spec Sheet 6865 D-2240-6892 Shore ATensile StrengthASTM D-412 Die C5,900psiElongation SetASTM D-412 Die C550%Elongation SetASTM D-412 Die C15%300% ModulusASTM D-412 Die C1,700psi100% ModulusASTM D-412 Die C750psiAbrasion LossDIN 53/51625mm3 Tear Die CASTM D-624660pliTear NickedASTM D-624360pliBayshore ResilenceASTM D-2632-751%Compression Set B 22 Hrs @ 70 CASTM D-395-69, Method B 9%Specific GravityASTM D-792, Method Specification SheetDISOGRIN 9250 PropertyStandardValueUnitsHardnessASTM D-2240-6892 Shore ATensile StrengthASTM D-412 Die C6,000psiElongation SetASTM D-412 Die C400%Elongation SetASTM D-412 Die C18%300% ModulusASTM D-412 Die C3,400psi100% ModulusASTM D-412 Die C1,600psiAbrasion LossDIN 53/51636mm3 Tear Die CASTM D-624700pliTear NickedASTM D-624480pliBayshore ResilenceASTM D-2632-735%Compression Set22 Hrs @ 70 CASTM D-395-69 (Method B)26%Specific GravityASTM D-792, Method.

2 DISOGRIN 9250 Material : Premium polyurethane, TODI basedType:CastColor:NaturalImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory Spec Sheet 9250 Specification SheetDISOGRIN D92 SName:DISOGRIN D92 SMaterial: Premium polyurethane, TODI basedType:Injection moldedColor:NaturalPropertyStandardValue UnitsImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory Spec Sheet D92S D-224094 3 Shore AHardnessASTM D-224043 3 Shore DTear StrengthASTM D-62445N/mm, StrengthASTM D-41225 MPa, @ 300% EnlongationASTM D-41215 MPa, D-412400% Set22 Hours @ 70 CASTM D-395 (Method B)30% Age (70 Hours @ 100 C)Change in HardnessASTM D-573 15 Change in Tensile StrengthASTM D-573 30% in ElongationASTM D-573-50% Resistance (70 Hours @ 100 C)Change in Hardness, astm D-471 10% in ValumeASTM D-471 15% Resistance, astm #1 Oil (70 Hours @ 100 C)Change in HardnessASTM D-471-5 to +15% MaxChange in Tensile StrengthASTM D-471-25% MaxChange in ElongationASTM D-471-45% in VolumeASTM D-471-10 to +5% Resistance, astm #3 Oil (70 Hours @ 100 C)

3 Change in HardnessASTM D-471-10 to +5% in StrengthASTM D-471-45% in ElongationASTM D-471-45% in VolumeASTM D-4710 to +25% Specification SheetDISOGRIN D80 SHardnessASTM D-224085 3 Shore ATear StrengthASTM D-62467N/mm, StrengthASTM D-41225 MPa, @ 300% EnlongationASTM D-4129 MPa, D-412400%, Set22 Hours @ 70 CASTM D-395 (Method B)35%, Age (70 Hrs @ 100 C)Change in HardnessASTM D-573 15 Shore AChange in Tensile StrengthASTM D-573 30% in ElongationASTM D-573-50% Resistance (70 Hrs @ 100 C)Change in Hardness, astm D-471 10% in ValumeASTM D-471 15% Resistance, astm #1 Oil (70 Hrs @ 100 C)Change in HardnessASTM D-471-5 to +15% MaxChange in Tensile StrengthASTM D-471-25% MaxChange in ElongationASTM D-471-45% MaxChange in VolumeASTM D-471-10 to +5% MaxFluid Resistance, astm #3 Oil (70 Hrs @ 100 C)Change in HardnessASTM D-471-10 to +5% in StrengthASTM D-471-45% in ElongationASTM D-471-45% :DISOGRIN D80 SMaterial: Premium polyurethane, TODI basedType:Injection moldedColor:NaturalPropertyStandardValue UnitsImportant Notes:Not to be used for Specification purposes.

4 These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory Spec Sheet D80S Specification SheetDISOGRIN 928 Name:DISOGRIN 928 Material : Premium polyurethane, TODI basedColor:NaturalPropertyStandardValueU nitsImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory Spec Sheet D928 5350598 2 Shore AHardnessDIN 5350560 5 Shore DSpecific GravityDIN 53512 25%Tensile StrengthDIN 53455 30N/mm2 Elongation at BreakDIN 53455 300%300% ModulusDIN 53455 28N/mm2 Tear StrengthDIN 53507 90N/mm2 WearDIN 53516 50mm3 Glass Transition-17 CLow Temperature Brittleness-50 CCompression Set24 Hrs @ 20 CDIN 53517 20%22 Hrs @ 70 CDIN 53517 35%70 Hrs @ 100 CDIN 53517 65% Material Specification SheetSIMRITAN 94 AU 925 Name:SIMRITAN 94 AU 925 Material : Premium polyurethane, TODI basedColor:BluePropertyStandardValueUnit sSpecific gravityDIN 5350594 Shore ARebound resilienceDIN 5351235%Modulus at 100%DIN strengthDIN elongationDIN 53504428%Compression Set22h @ 70 CDIN 5351740%Important Notes:Not to be used for Specification purposes.

5 These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory. The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Spec Sheet 94AU925 Spec Sheet Simritan 98 AU 928 gravityDIN 5350597 Shore AModulus at 100 %DIN strengthDIN elongationDIN 53504389% Material Specification SheetSIMRITAN 98 AU 928 Name:SIMRITAN 98 AU 928 Material : Premium polyurethane (TODI based)Color:BlueImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory. The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Specification SheetNOVATHAN 95 AU V142 Name:NOVATHAN 95 AU V142 Material : Premium polyurethane, MDI basedColor:BluePropertyStandardValueUnit sDurometer hardnessASTM D-224095 2 Shore ADurometer hardnessASTM D-224048 3 Shore DDensityASTM strengthASTM D-41240N/mm2 Elongation at breakASTM D-412500%Tear strengthASTM D-624120N/mmRebound resilienceDIN 5351242%AbrasionDIN 5351618mm3 Compression set70h/70 C, 25% compressionASTM D-395 (Method B)27%Compression set24h/100 C, 25% compressionASTM D-395 (Method B)24%Compression Set70h/70 C, 25% compressionASTM D-395 (Method B)26%Important Notes:Not to be used for Specification purposes.

6 These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory. The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Spec Sheet NOVATHAN Specification SheetMerkel 70 NBR B209 Name:Merkel 70 NBR B209 Material : NBR (Acrylonitrile Bunadiene Rubber) g/cm3 Hardness70 5 SHORE AHardness70 5 IRHDT ensile Strength 11N/MMUltimate Elongation 250%Modulus 100% Elongation* 2 Tear Strength*11N/mmChange In Volume* astm Oil I (168 hr/100 C) Oil III (168 hr/100 C)13%Change In Hardness* astm Oil I (168 hr/100 C)1 PointASTM Oil III (168 hr/100 C)-8 PointCompression Set24 hr/70 CDIN 53517 11%70 hr/100 CDIN 53517 23%24 hr/70 CASTM D 395 B 10%70 hr/100 CASTM-D 395 B 15%*Typical PropertiesImportant Notes:Not to be used for Specification purposes.

7 These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory. The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Spec Sheet 70 NBR B209 Specification SheetMerkel 70 NBR B276 Name:Merkel 70 NBR B276 Material : NBR (Acrylonitrile Bunadiene Rubber)Color:BlackPropertyStandardValueU nitsDensityDIN g/cm3 HardnessDIN 5350570 5 Shore AHardnessDIN 5351973 5 IRHDT ensile StrengthDIN 53504 14N/mm2 Ultimate ElongationDIN 53504 280%Modulus 100% ElongationDIN 535045N/mm2 Resistance To Tear PropagationDIN 5351518N/mm2 Low Temperature Reference Value TRDIN 53520-22 CBrittle Point TSDIN 53546-50 CChange In VolumeASTM Oil I (168 hr/100 C)-5% astm Oil III (168 hr/100 C)11%Change In HardnessASTM Oil I (168 hr/100 C)5 PointsASTM Oil III (168 hr/100 C)-6 PointsCompression Set24 hr /70 CDIN 53517 17%70 hr /100 CDIN 53517 32%24 hr /70 CASTM-D 395 B 12%70 hr /100 CASTM-D 395 B 20%Important Notes:Not to be used for Specification purposes.

8 These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory. The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Spec Sheet 85 NBR 70 B276 Spec Sheet Simrit 72 NBR 872 gravityDIN 5350572 Shore ARebound resilienceDIN 5351234%Modulus at 100 %DIN strengthDIN elongationDIN 53504270%Compression set (22 hr/100 C)DIN 5351720% Material Specification SheetMerkel 72 NBR 872 Name:Merkel 72 NBR 872 Material : NBR (Acrylonitrile Bunadiene Rubber)Color:BlackImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory.

9 The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Specification SheetMerkel 79 NBR B246 Name:Merkel 79 NBR B246 Material : NBR (Acrylonitrile Bunadiene Rubber)Color:BlackPropertyStandardValueU nitsDensityDIN g/cm3 HardnessDIN 5350578 5 Shore AHardnessDIN 5351978 5 IRHDT ensile StrengthDIN 53504 ElongationDIN 53504 250%Modulus 100% Elongation*DIN Strength*DIN 5351516N/mmChange In Volume* astm Oil I (168 hr/100 C) Oil III (168 hr/100 C)16%Change In Hardness* astm Oil I (168 hr/100 C)2 PointsASTM Oil III (168 hr/100 C)-12 PointsCompression Set24 hr/70 CDIN 53517 15%70 hr/100 CDIN 53517 40%24hr/70 CASTM-D 395 B 14%70 hr/100 CASTM-D 395 B 26%*Typical PropertiesImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory.

10 The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Spec Sheet 79 NBR B246 Spec Sheet Simrit 80 NBR 709 gravityDIN 5350582 Shore ARebound resilienceDIN 5351229%Modulus at 100 %DIN strengthDIN elongationDIN 53504290%Compression set (22 hr/100 C)DIN 5351725% Material Specification SheetMerkel 80 NBR 709 Name:Merkel 80 NBR 709 Material : NBR (Acrylonitrile Bunadiene Rubber)Color:BlackImportant Notes:Not to be used for Specification purposes. These values serve only as a guide for engineering design. Values aremedian values obtained from laboratory specimens. The given values are based on a limited number of tests onstandard test pieces (2mm sheets) produced in the laboratory. The data of finished parts can deviate from abovevalues depending on the manufacturing process and the component Spec Sheet Simrit 80 NBR 878 gravityDIN 5350583 Shore ARebound resilienceDIN 5351226%Modulus at 100 %DIN strengthDIN elongationDIN 53504170%Compression set (22 hr/100 C)DIN 5351720% Material Specification SheetMerkel 80 NBR 878 Name:Merkel 80 NBR 878 Material : NBR (Acrylonitrile Bunadiene Rubber)Color:BlackImportant Notes:Not to be used for Specification purposes.