MATERIAL TECHNICAL DATASHEET CARBON STEEL CK 75 …

CARBON STEEL CK 75 FOR CUTTING TWEEZERS (ORD) MATERIAL number ( aisi 1075) COMPOSITIONCSiMnPSCrMoNiWt % - - - MADE PRECISION INSTRUMENTS100% MANUFACTURED IN Switzerland Box 264 Viale Serfontana 11CH-6834 Morbio InferioreSwitzerlandtel +41 91 683 55 37fax +41 91 683 93 91 MATERIAL TECHNICAL DATASHEETT echnical information are provided to the best of Regine Switzerland SA knowledge and average values obtained from laboratory s test made on the Switzerland SA declines all responsability from an improper application or use of the product described in this documents. MECHANICAL PROPERTIES AND HOT FORMINGS tateSoft AnnealedHardened + TemperedHardness HB30 210371 - 525 Hardness Rockwell B 95 Hardness Rockwell C 40 - 53 Tensile strength (N/mm2) 6401320 - 1870 Elongation after fracture (Lo = 5do) 6 Elongation after fracture (Lo = 80 mm) 12%

CARBON STEEL CK 75 FOR CUTTING TWEEZERS (ORD) Material number 1.1248 (AISI 1075) COMPOSITION C Si Mn P S Cr Mo Ni Wt % 0.70-0.80 0.15-0.35 0.60-0.90 ≤ …

Tags:

  Steel, Carbon, 1057, Aisi, Carbon steel ck 75, Aisi 1075

Information

Domain:

Source:

Link to this page:

Please notify us if you found a problem with this document:

Other abuse

Advertisement

Transcription of MATERIAL TECHNICAL DATASHEET CARBON STEEL CK 75 …

1 CARBON STEEL CK 75 FOR CUTTING TWEEZERS (ORD) MATERIAL number ( aisi 1075) COMPOSITIONCSiMnPSCrMoNiWt % - - - MADE PRECISION INSTRUMENTS100% MANUFACTURED IN Switzerland Box 264 Viale Serfontana 11CH-6834 Morbio InferioreSwitzerlandtel +41 91 683 55 37fax +41 91 683 93 91 MATERIAL TECHNICAL DATASHEETT echnical information are provided to the best of Regine Switzerland SA knowledge and average values obtained from laboratory s test made on the Switzerland SA declines all responsability from an improper application or use of the product described in this documents. MECHANICAL PROPERTIES AND HOT FORMINGS tateSoft AnnealedHardened + TemperedHardness HB30 210371 - 525 Hardness Rockwell B 95 Hardness Rockwell C 40 - 53 Tensile strength (N/mm2) 6401320 - 1870 Elongation after fracture (Lo = 5do) 6 Elongation after fracture (Lo = 80 mm) 12%


Related search queries