Minimization of the Casting Defects Using …
International Journal of Engineering Science Invention ISSN (Online): 2319 6734, ISSN (Print): 2319 6726 ||Volume 5 Issue 12|| December 2016 || PP. 06-10 6 | Page Minimization of the Casting Defects Using Taguchi s Method Harvir Singh1, Aman Kumar2 1(Mechanical Engineering Department, Maharana Pratap College of Technology, Gwalior /RGPV, Bhopal, India) 2(Mechanical Engineering Department, College of Science & Engineering Jhansi (UP), /AKTU, Lucknow, India) Abstract: This paper is relates with Casting Defects like pinholes, scabs, sand holes, slag, mould shifting, parting line Defects , runner & riser Defects which mainly occurs in valve Casting in foundry.
Minimization Of The Casting Defects Using Taguchi’s Method www.ijesi.org 7 | Page Joseph I. Achebo [21] In this research study, the structural steel failure problems encountered by a multi-
Download Minimization of the Casting Defects Using …
Information
Domain:
Source:
Link to this page:
Please notify us if you found a problem with this document:
Related search queries
Minimization, Defects, Casting defects, Aluminum, Casting, Of casting defects, International Journal of Engineering Research, International Journal of Engineering Research and General Science, Shrinkage defect, Defects Shrinkage defect, And Minimization of Surface Defects on, Defects by increasing the surface temperature, Defects by increasing the surface temperature during, Analysis of parameters for casting, Minimization of Casting Defects