WELDING DEFECTS

following defects:-: –Cavity –Shrinkage cavity –Slag inclusion –Undercut Green • Slight variation from homogeneity in the form of one or more of the following defects:- –Gas cavity –Shrinkage cavity –Slag inclusion –Undercut –Incomplete penetration 16/06/2015 17