Photoelectron spectroscopy for surface analysis: X-ray and ...
diposit.ub.eduPhotoelectron spectroscopy for surface analysis 2 MT.1 The kinetic energy of the emitted electron depends on the energy of the photon, which is given by Einstein’s photoelectric law KE=hv–BE , where BE is the binding energy of the atomic orbital from which the electron originates, hv is the