Tensile test Through thickness tensiletest (1) Charpy V-notch impact test Min. yield strength R e [MPa] Tensile strength R m Min. reduction of a reaZ z Longitudinal di ection Transverse di tion Nominal thickness(mm ) [MPa] ≤ 16 > 16 ≤ 40 HISTAR 355 TZ OFFSHORE 355 355 460-620-40° C KV ≥50 J HISTAR 355 TZK OFFSHORE 355 355 460-620-40° C ...