of submerged arc or electroslag fluxes, can absorb mois-ture, depending on storage conditions and handling prac-tices. To limit hydrogen content in deposited welds, welding consumables must be properly maintained, and welding must be performed on surfaces that are clean and dry. The second necessary condition for heat affected zone